The five defects that account for most logo rejections at inspection, and the control that removes each one. Print cracks or peels after washing Cause: wrong ink or transfer on a stretch or coated fabric. Control: method chosen from the compatibility chart above; 40+ wash test on the sample before approval. Embroidery puckers the panel Cause: stitch density too high for the fabric weight. Control: density set at 4–5 stitches/mm with a tear-away backing on fabrics under 420D. Colour drifts from the Pantone Cause: mixing by eye. Control: inks and threads matched to a physical Pantone chip; lab dip approved before bulk. See materials & colours . Logo sits 1 cm off between bags Cause: free-hand placement. Control: laser-marked jig per style, ±3 mm checked at inline inspection . Patch peels at the corner Cause: bond temperature or time too low. Control: 150–170 °C for 10–15 s on a calibrated press, plus edge stitching on patches over 5 cm. Logo too small to read on Amazon thumbnails Cause: logo scaled from a print file. Control: we advise a minimum 6 cm mark on the main panel for FBA listings and photograph it free on production orders. Factory
reflective.